Cad é ábhar A672 C65

Cad é ábhar A672 C65?

A672 GrC65 CL22‌ belongs to the carbon-manganese-silicon steel series. Its chemical composition is meticulously designed, with carbon content controlled below 0.22%, manganese content between 1.0-1.5%, and appropriate silicon added to enhance strength and toughness. This alloy formulation enables the steel pipe to maintain good plasticity while possessing high yield strength (>415MPa) agus neart teanntachta (Níos mó ná nó cothrom le 485MPa).

Is díol suntais go háirithe, tar éis dul faoi phróisis rollta agus fuaraithe rialaithe speisialta, go n-éiríonn leis an ábhar éifeachtaí scagtha gráin suntasacha agus cruas tionchair íseal teochta den scoth, a chomhlíonann riachtanais seirbhíse go hiomlán ag -46 céim . Maidir le friotaíocht creimeadh, trí eilimintí micrea-chóimhiotail a chur leis agus rialú docht ar ábhar sulfair agus fosfair, comhlíonann a fhriotaíocht HIC (Scáineadh Ionduchtaithe Hidrigin) agus SSC (Creimeadh Creimthe Strus Sulfíd) caighdeáin NACE MR0175, rud a fhágann go bhfuil sé oiriúnach go háirithe do choinníollacha oibriúcháin crua ina bhfuil suilfíd hidrigine.

 

Astm a672 gr c65 sonraíocht pdf

Sonraíocht Chaighdeánach A516-65
Cóid agus Caighdeáin

ANSI, ASME, ASTM, API, SAE, BS, AGA, AWWA, ISO, DIN

Toisí ASME/ ANSI B36.10 / 19
Méid Caighdeánach 1/2" NB go 36" NB (LSAW, SSAW, HSAW)
Tiús Balla 3-12mm
Sceidil píopaí SCH 5, SCH10, SCH 40, SCH 80, SCH 80S, SCH 160, SCH XXS, SCH XS
Teicnící táirgthe Gan uaim / ERW / Táthaithe / Déanta / CDW / EFW
Cruthanna ar Fáil Cruth Babhta, Leathbhabhta, Cearnóg, Dronuilleogach nó Saincheaptha
TEICNÍC UO (UOE), JCO (JCOE, COE)
Fad 3 go Uasmhéid 18 Méadair nó saincheaptha
Deireadh Píob Deireadh Beveled, Deireadh Gnáth, Treaded
Deimhniú Tástála Muileann GA 10204/3.1B

 

Astm a672 gr c65 toisí

NB Méid OD 40S 5S 10S S10 S20 S40 S60 XS/80S S80 S100 S120 S140 S160 XXS
mm mm mm mm mm mm mm mm mm mm mm mm mm mm mm
  1/8" 10.29     1.2     1.73     2.41          
  1/4" 13.72     1.7     2.24     3.02          
  3/8" 17.15     1.7     2.31     3.2          
15 1/2" 21.34 2.8 1.7 2.1     2.77   3.73 3.73       4.78 7.47
20 3/4" 26.67 2.9 1.7 2.1     2.87   3.91 3.91       5.56 7.82
25 1" 33.4 3.4 1.7 2.8     3.38   4.55 4.55       6.35 9.09
32 1 1/4" 42.16 3.6 1.7 2.8     3.56   4.85 4.85       6.35 9.7
40 1 1/2" 48.26 3.7 1.7 2.8     3.68   5.08 5.08       7.14 10.2
50 2" 60.33 3.9 1.7 2.8     3.91   5.54 5.54       9.74 11.1
65 2 1/2" 73.03 5.2 2.1 3.1     5.16   7.01 7.01       9.53 14
80 3" 88.9 5.5 2.1 3.1     5.49   7.62 7.62       11.1 15.2
90 3 1/2" 101.6 5.7 2.1 3.1     5.74   8.08 8.08          
100 4" 114.3 6 2.1 3.1     6.02   8.56 8.56   11.1   13.5 17.1
125 5" 141.3 6.6 2.8 3.4     6.55   9.53 9.53   12.7   15.9 19.1
150 6" 168.3 7.1 2.8 3.4     7.11   10.97 11   14.3   18.3 22
200 8" 219.1 8.2 2.8 3.8   6.4 8.18 10.3 12.7 12.7 15.1 19.3 20.6 23 22.2
250 10" 273.1 9.3 3.4 4.2   6.4 9.27 12.7 12.7 15.1 19.3 21.4 25.4 28.6 25.4
300 12" 323.9 9.5 4 4.6   6.4 10.3 14.3 12.7 17.5 21.4 25.4 28.6 33.3 25.4
350 14" 355.6 9.5 4 4.8 6.4 7.9 11.1 15.1 12.7 19.1 23.8 27.8 31.8 35.7  
400 16" 406.4 9.5 4.2 4.8 6.4 7.9 12.7 16.7 12.7 21.4 26.2 31 36.5 40.5  
450 18" 457.2 9.5 4.2 4.8 6.4 7.9 14.3 19.1 12.7 23.8 29.4 34.9 39.7 45.2  
500 20" 508 9.5 4.8 5.5 6.4 9.5 15.1 20.6 12.7 26.2 32.5 38.1 44.5 50  
550 22" 558.8 9.5 4.8 5.5 6.4 9.5   22.2 12.7 28.6 34.9 41.3 47.6 54  
600 24" 609.6 9.5 5.5 6.4 6.4 9.5 17.5 24.6 12.7 31 38.9 46 52.4 59.5  
650 26" 660.4 9.5     7.9 13     12.7            
700 28" 711.2 9.5     7.9 13     12.7            
750 30" 762 9.5 6.4 7.9 7.9 13     12.7            
800 32" 812.8 9.5     7.9 13 17.5   12.7            
850 34" 863.6 9.5     7.9 13 17.5   12.7            
900 36" 914.4 9.5     7.9 13 19.1   12.7  

 

A672 Gr.C65 VSA672 Gr.C60

Paraiméadar A672 Gr.C65 A672 Gr.C60
Comhdhéanamh Ceimiceach    
● Carbón (C) Níos lú ná nó cothrom le 0.22% Níos lú ná nó cothrom le 0.22%
● Mangainéis (Mn) 1.0-1.5% 0.85-1.35%
● Sileacan (Si) 0.15-0.40% 0.15-0.40%
Airíonna Meicniúla    
● Neart Táirgeachta >415 MPa (60 ksi) Níos mó ná nó cothrom le 415 MPa (60 ksi)
● Neart Teanntachta Níos mó ná nó cothrom le 485 MPa (70 ksi) 485-690 MPa (70-100 ksi)
● Íseal-Teagacht Teochta (-46 céim ) Níos mó ná nó cothrom le 34J (NACE MR0175) Níos mó ná nó cothrom le 27J
Saintréithe Próiseála    
● Cóireáil Teasa TMCP (Próiseas Rialaithe Teirmmeicniúil) Normalú traidisiúnta
● Méid Grán Grád 8-9 (ASTM E112) Grád 7-8
Friotaíocht Creimthe    
● Tástáil HIC/SSC Gabhann sé NACE TM0284/TM0177 Roghnach
● Pcm Carbóin Coibhéiseach 0.23-0.25 0.25-0.28
Cúrsaí Eacnamaíochta    
● Costas Ábhar +15-20% Praghas Bunlíne
● Saol Seirbhíse 25+ bliain (seirbhís ghéar) 15-20 bliain

 

Monarcha Píob Táthaithe A672 GR C65