ASTM A671 CJF115 Class 11 Steel Pipe

1. What is ASTM A671 CJF115 Class 11?

low-temperature service (-115℃F/-81.7℃)

Class 11: 11,000 psi (76 MPa)

:

"CJF115"=Charpy V-notch testing at -115℃F (min. 17 ft-lb/23 J)

Single-normalized heat treatment

2. Where is it typically used?

:

:

Low-to-medium pressure gas distribution

3. Material properties?

:

Tensile: >=65 ksi (448 MPa)

Yield: >=40 ksi (276 MPa)

:

-115℃F

Min. elongation: 22%

:

Carbon: <=0.28%

S/P <=0.030%

4. Manufacturing process?

:

Standard EFW with post-weld normalization

:

11,000 psi (76 MPa)

NDE: RT or UT (100% coverage)

:

5. Fabrication requirements?

:

Preheat: 250–450℃F (121–232℃)

:

Cold bending (min. 7D radius)

: