1. What is ASTM A671 CJB115 Class 13 steel pipe?
ASTM A671 CJB115 Class 13 is an electric-fusion-welded (EFW) carbon steel pipemoderate-to-high pressure industrial applications (typically operating above -20℃F/-29℃). The "Class 13" designation indicates a minimum yield strength of 13 ksi (90 MPa), offering enhanced performance over lower classes in the CJB115 series.
2. Key specifications and material properties?
CJB115 carbon steel (higher carbon than CJA grades)
>=13 ksi (90 MPa)
60-80 ksi (414-552 MPa)
Carbon (C): <=0.35%
Manganese (Mn): <=1.35%
Phosphorus/Sulfur (P/S): <=0.035%
3. Typical industrial applications?
Medium-pressure fluid systems
Structural supports in moderate-stress environments
4. How does it compare to adjacent classes?
| 12 | 12 ksi | |
| 13 | 13 ksi | |
| 15 | 15 ksi | Higher-pressure industrial |
5. Fabrication and quality control requirements?
Standard procedures with preheat recommended for thickness >1" (25.4 mm)
Hydrostatic test at 1.5x design pressure (mandatory)
Visual and dimensional checks per ASTM A671