Píobán ASTM A358 EFW
Is píopa cruach cóimhiotal cróimiam-nicil austenític austenític táthaithe é A358 le haghaidh úsáide ardteochta agus is caighdeán sonraíochta níos déine é ná an caighdeán A312.
Is soláthraí gairmiúil Píopaí agus Feadáin Táthaithe Electro Fusion Cruach Dhosmálta é GNEE Group, soláthraímid raon leathan táirgí lena n-áirítear 304, 304L, 304H, 309, 309S, 310,310S, 316, 316L, 316H, 317L,1321, H. ,904 agus mar sin de. Is féidir leat teagmháil a dhéanamh linn ag am ar bith más gá duit.
Sonraíocht Píobáin A358 EFW
| Caighdeán |
ASTM, DIN, JIS, GB, AISI, ISO, etc Caighdeáin Idirnáisiúnta eile |
| Toisí |
ASTM, ASME, agus API |
| Sonraíochtaí |
ASTM A358 / ASME SA 358 - Aicme 1, Aicme 3, Aicme 2, Aicme 4, Aicme 5 |
| Grád |
TP 304, TP 304L/H, TP 304LN, TP 316L, TP 316, TP 321/H, TP 347/H |
| Méid |
8" NB go 72" NB. |
| Tiús |
3mm go 60mm |
| Fad |
Suas le 6 méadar, faid gearrtha saincheaptha |
| Tiús bhalla |
3mm go 20mm, SCH 5/5S, 10/10S, 20/20S, 40/40S, 80/80S, 120/120S, 160/160S de réir ANSI B36.19/36.10 |
| Críochnaigh |
Uimh.1 Críochnaigh Piocáilte, Críochnaigh BA, bailchríoch Uimh.4, Píopaí Cruach Gan uaim Electropolished |
| Coinníoll Seachadta |
Críoch Te, Críoch Fuar, Geal Annealed, Annealed agus picilte, Snasta, Passivated, Strus Athbheochan |
| Iarratas |
Tionscal Bia & Dí, Núicléach, Tionscal Foirgníochta, Gléasraí Teirmeacha & Cumhachta, Peitriceimiceach, Coirí, Tionscal Stroighne, Gléasraí Geoiteirmeacha, Poist Ionstraimíochta, Poist Mheicniúla, Malartóirí Teasa, Trealamh Ola agus Gáis agus Oibreacha Píobáin |
| Pacáiste |
Bundles cruach, caipíní plaisteacha ag an dá cheann, málaí fite nó ar iarratas |
Comhdhéanamh Ceimiceach Píopa Cruach Dhosmálta A358
| A358 GRÁID |
UNS |
C |
Mn |
P |
S |
Si |
Cr |
Ni |
Mo |
Ti |
Nb |
N |
| TP304 |
S3040 |
0.08 |
2.0 |
0.045 |
0.030 |
1.0 |
18.0-20.0 |
8.0-11.0 |
|
|
|
|
| TP304L |
0.035 |
|
2.0 |
0.045 |
0.030 |
1.0 |
18.0-20.0 |
8.0-13.0 |
|
|
|
|
| TP304H |
S30409 |
0.04-0.10 |
2.0 |
0.045 |
0.030 |
1.0 |
18.0-20.0 |
8.0-11.0 |
|
|
|
|
| TP304N |
S30451 |
0.08 |
2.0 |
0.045 |
0.030 |
1.0 |
18.0-20.0 |
8.0-18.0 |
|
|
|
0.10-0.16 |
| TP304LN |
S30453 |
0.035 |
2.0 |
0.045 |
0.030 |
1.0 |
18.0-20.0 |
8.0-12.0 |
|
|
|
0.10-0.16 |
| ASME SA358 TP309S |
S30908 |
0.08 |
2.0 |
0.045 |
0.030 |
1.0 |
22.0-24.0 |
12.0-15.0 |
0.75 |
|
|
|
| ASME SA358 TP309H |
S30909 |
0.04-0.10 |
2.0 |
0.045 |
0.030 |
1.0 |
22.0-24.0 |
12.0-15.0 |
|
|
|
|
| ASME SA358 TP309Cb |
S30940 |
0.08 |
2.0 |
0.045 |
0.030 |
1.0 |
22.0-24.0 |
12.0-16.0 |
0.75 |
|
10xC min 1.10 max |
|
| ASME SA358 TP309HCb |
S30941 |
0.04-0.10 |
2.0 |
0.045 |
0.030 |
1.0 |
22.0-24.0 |
12.0-16.0 |
0.75 |
|
10xC min 1.10 nmax |
|
| ASME SA358 TP310S |
S3108 |
0.08 |
2.0 |
0.045 |
0.030 |
1.0 |
24.0-26.0 |
19.0-22.0 |
0.75 |
|
|
|
| ASME SA358 TP310H |
S3109 |
0.04-0.10 |
2.0 |
0.045 |
0.030 |
1.0 |
24.0-26.0 |
19.0-22.0 |
|
|
|
|
| ASME SA358 TP310Cb |
S31040 |
0.08 |
2.0 |
0.045 |
0.030 |
1.0 |
24.0-26.0 |
19.0-22.0 |
0.75 |
|
10xC min 1.10 max |
|
| ASME SA358 TP310HCb |
S31041 |
0.04-0.10 |
2.0 |
0.045 |
0.030 |
1.0 |
24.0-26.0 |
19.0-22.0 |
0.75 |
|
10xC min 1.10 max |
|
| ASME A358 TP316 |
S3160 |
0.08 |
2.0 |
0.045 |
0.030 |
1.0 |
16.0-18.0 |
11.0-14.0 |
2.0-3.0 |
|
|
|
| ASTM SA358 TP316L |
S31603 |
0.035 |
2.0 |
0.045 |
0.030 |
1.0 |
16.0-18.0 |
10.0-14.0 |
2.0-3.0 |
|
|
|
| ASTM SA358 TP316H |
S31609 |
0.04-0.10 |
2.0 |
0.045 |
0.030 |
1.0 |
16.0-18.0 |
11.0-14.0 |
2.0-3.0 |
|
|
|
| TP316Ti |
S31635 |
0.08 |
2.0 |
0.045 |
0.030 |
0.75 |
16.0-18.0 |
10.0-14.0 |
2.0-3.0 |
5x (C-N) -0.70 |
|
0.10 |
| TP316N |
S31651 |
0.08 |
2.0 |
0.045 |
0.030 |
1.0 |
16.0-18.0 |
10.0-14.0 |
2.0-3.0 |
|
|
0.10-0.16 |
| TP316LN |
S31653 |
0.035 |
2.0 |
0.045 |
0.030 |
1.0 |
16.0-18.0 |
11.0-14.0 |
2.0-3.0 |
|
|
0.10-0.16 |
| ASME SA358 TP317 |
S3170 |
0.08 |
2.0 |
0.045 |
0.030 |
1.0 |
18.0-20.0 |
10.0-14.0 |
3.0-4.0 |
|
|
|
| ASME SA358 TP317L |
S31703 |
0.035 |
2.0 |
0.045 |
0.030 |
1.0 |
18.0-20.0 |
11.0-15.0 |
3.0-4.0 |
|
|
|
| TP321 |
S3210 |
0.08 |
2.0 |
0.045 |
0.030 |
1.0 |
17.0-19.0 |
9.0-12.0 |
|
|
|
0.10 |
| TP321H |
S32109 |
0.04-0.10 |
2.0 |
0.045 |
0.030 |
1.0 |
17.0-19.0 |
9.0-12.0 |
|
|
|
0.10 |
| TP347 |
S3470 |
0.08 |
2.0 |
0.045 |
0.030 |
1.0 |
17.0-19.0 |
9.0-13.0 |
|
|
|
|
| TP347H |
S34709 |
0.04-0.10 |
2.0 |
0.045 |
0.030 |
1.0 |
17.0-19.0 |
9.0-13.0 |
|
|
|
|
| TP347LN |
S34751 |
0.05-0.02 |
2.0 |
0.045 |
0.030 |
1.0 |
17.0-19.0 |
9.0-13.0 |
|
|
0.20- 50.0 |
0.06-0.10 |
| TP348 |
S3480 |
0.08 |
2.0 |
0.045 |
0.030 |
1.0 |
17.0-19.0 |
9.0-13.0 |
|
|
|
|
| ASME SA358 TP348H |
S34809 |
0.04-0.10 |
2.0 |
0.045 |
0.030 |
1.0 |
17.0-19.0 |
9.0-13.0 |
|
|
|
|
Píopaí Cruach ASME SA358 EFW Airíonna Meicniúla
| Ábhar |
Teas |
Teocht |
Neart Teanntachta |
Neart Toradh |
Fadú %, Íosmhéid |
| Cóireáil |
Min. |
Ksi (MPa), Min. |
Ksi (MPa), Min. |
| |
º F(º C) |
|
|
| TP304 |
Réiteach |
1900 (1040) |
75(515) |
30(205) |
35 |
| TP304L |
Réiteach |
1900 (1040) |
70(485) |
25(170) |
35 |
| TP316 |
Réiteach |
1900(1040) |
75(515) |
30(205) |
35 |
| TP316L |
Réiteach |
1900(1040) |
70(485) |
25(170) |
35 |
Caoinfhulaingt Píopaí Cruach ASTM A358
| Ainmneoir NPS |
Athruithe Ceadaithe sa Trastomhas Lasmuigh |
| Thar I. |
Faoi In. |
| 1/8 go 1-1/2, lena n-áirítear |
1/64 (0.015) |
1/32 (0.031) |
| Níos mó ná 1-1/2 go 4, lena n-áirítear |
1/32 (0.031) |
1/32 (0.031) |
| Níos mó ná 4 go 8, lena n-áirítear |
1/16 (0.062) |
1/32 (0.031) |
| Os cionn 8 go 18, lena n-áirítear |
3/23 (0.093) |
1/32 (0.031) |
Tiús Balla Ainmniúil
| Ainmneoir NPS |
Trastomhas Lasmuigh i. |
Sceideal 5S in. |
Sceideal 10S in. |
Sceideal 40S in. |
Sceideal 80S in. |
| 1/4 |
0.540 |
|
0.065 |
0.088 |
0.119 |
| 3/8 |
0.675 |
|
0.065 |
0.091 |
0.126 |
| 1/2 |
0.840 |
0.065 |
0.083 |
0.109 |
0.147 |
| 3/4 |
1.050 |
0.065 |
0.083 |
0.113 |
0.154 |
| 1.0 |
1.315 |
0.065 |
0.109 |
0.133 |
0.179 |
| 1 1/4 |
1.660 |
0.065 |
0.109 |
0.140 |
0.191 |
| 1 1/2 |
1.900 |
0.065 |
0.109 |
0.145 |
0.200 |
| 2 |
2.375 |
0.065 |
0.109 |
0.154 |
0.218 |
| 2 1/2 |
2.875 |
0.083 |
0.120 |
0.203 |
0.276 |
| 3 |
3.500 |
0.083 |
0.120 |
0.216 |
0.300 |
| 3 1/2 |
4.000 |
0.083 |
0.120 |
0.226 |
0.318 |
| 4 |
4.500 |
0.083 |
0.120 |
0.237 |
0.337 |
| 5 |
5.563 |
0.109 |
0.134 |
0.258 |
0.375 |
| 6 |
6.625 |
0.109 |
0.134 |
0.280 |
0.432 |
| 8 |
8.625 |
0.109 |
0.148 |
0.322 |
0.500 |
| 10 |
10.750 |
0.134 |
0.165 |
0.365 |
0.500 |
| 12 |
12.750 |
0.156 |
0.180 |
0.375 |
0.500 |
Caoinfhulaingt Balla Píob Cruach ASTM A358
| NPS |
Caoinfhulaingt Píobán Cruach ASTM A358, % |
| + |
– |
| 1/8-2 1 /2 |
20.0 |
12.5 |
| 3~18, t/D Níos lú ná nó cothrom le 5% |
22.5 |
12.5 |
| 3~18, t/D> 5% |
15.0 |
12.5 |
| Níos mó ná nó cothrom le 20, táthaithe |
17.5 |
12.5 |
| Níos mó ná nó cothrom le 20, gan uaim, t/D Níos lú ná nó cothrom le 5% |
22.5 |
12.5 |
| ≥ 20, seamless, t/D> 5% |
15.0 |
12.5 |
Soláthar GNEE Píopa Táthaithe Cruach Dhosmálta A358