Píobán Cruach ASTM A691 Grád 11 22 91 LSAW
video

Píobán Cruach ASTM A691 Grád 11 22 91 LSAW

Cinneann sonraíochtaí píopa tréithe éagsúla na miotail, mar shampla comhdhéanamh ceimiceach, airíonna meicniúla, agus toisí.
Glaoigh Linn
Chatear nu'bya
Réamhrá Táirgí

Caighdeán: ASTM A691/ASTM SA691
Gráid: CM{0}} CM-70 CM-75 CMSH-70CMS-75 CMSH-801/2 CR 1CR 1-1/4 CR 2-1/4 CR 3CR 5CR 9CR 91
Aicme: Aicme 10,11,12,13,20,21,22,23,30,31,32,33,40,41,42,43
Méid: 1/2"~60"

Caighdeán

ASTM A691

Toisí ASME/ ANSI B36.10 / 19
Méid Caighdeánach 1/2" NB go 60" NB (ERW, EFW, LSAW, SSAW, HSAW)
Tiús Balla 3-12mm
Cruthanna ar Fáil Cruth Babhta, Leathbhabhta, Cearnóg, Dronuilleogach nó Saincheaptha
Fad 3 go Uasmhéid 18 Méadair nó saincheaptha
Deireadh Píob Deireadh Beveled, Deireadh Gnáth, Treaded
Deimhniú Tástála GA 10204 3.1 B
Grád Píob Sonraíocht ASTM Raon Teochta Teasa-Chóireála Iar-Weld (Faoiseamh ar Shráideanna), F(C) Teocht a normalú, uas mura dtugtar a mhalairt faoi deara, F (C) Teocht Múchadh, uas mura luaitear a mhalairt, F (C) Teocht Teochta, nóim, F(C)
CM-65 A204/ A204M 1100 go 1200 (590 go 650) 1700 (925)
CM-70 A204/ A204M 1100 go 1200 (590 go 650) 1701 (925)
CM-75 A204/ A204M 1100 go 1200 (590 go 650) 1702 (925)
CMSH-70 A537/A 537M 1100 go 1200 (590 go 650) 1703 (925)
CMS-75 A 299/A 299M 1100 go 1200 (590 go 650) 1704 (925)
CMSH-80 A537/A 537M 1100 go 1200 (590 go 650) A 1700 (925) 1100 go 1250 (590 go 675)
1/2 CR A387 / A387M 1100 go 1300 (590 go 705) 180 (1010) 1700 (925) 1150 go 1375 (620 go 745)
1CR A387 / A387M 1100 go 1350 (590 go 730) 181 (1010) 1700 (925) 1150 go 1375 (620 go 745)
1-1/4 CR A387 / A387M 1100 go 1375 (590 go 745) 182 (1010) 1700 (925) 1150 go 1375 (620 go 745)
2-1/4 CR A387 / A387M 1200 go 1400 (650 go 760) 183 (1010) 1700 (925) 1250 go 1400 (675 go 760)
3CR A387 / A387M 1200 go 1400 (650 go 760) 184 (1010) 1700 (925) 1250 go 1400 (675 go 760)
5CR A387 / A387M 1200 go 1400 (650 go 760) 185 (1010) 1700 (925) 1300 go 1400 (705 go 760)
9CR A387 / A387M 1325 go 1375 (715 go 745) B 1325 go 1375 (715 go 745)
91 A387 / A387M 1350 go 1420 (730 go 770) 1350 go 1420 (730 go 770) 1900 nóim (1040 nóim) 1350 go 1440 (730 go 780)

 

Clibeanna Te: píopa cruach astm a691 grád 11 22 91 lsaw, an tSín astm a691 grád 11 22 91 monaróirí píopa cruach lsaw, soláthraithe