Apr 02, 2024 Fág nóta

ASTM A252 Grád 3 Píopa Píopa

Cur síos ar Tháirgí

Carn píopa cruach soláthair GNEE i gcaighdeán ASTM A252 mar atá thíos na coinníollacha:
Gráid: 1, 2, agus 3
Toisí: Suas le 48 orlach gan uaim agus táthaithe

Cineálacha: Gan uaim, Táthaithe (ERW, LSAW, SSAW, DSAW)
Tiús: Sceideal STD, 40, XS, 80, XXS, 160
Fad: 6m, 12m nó saincheaptha.
Críoch: Beveled, Plain
Cóireáil Bratuithe: FBE, 3PE, Galvanized

Airíonna meicniúla de chaighdeán ASTM a252

Grád

Grád 1

Grád 2

Grád 3

Neart Teanntachta, Min psi

50,000

60,000

66,000

Neart Toradh, Min psi

30,000

35,000

45,000

Cairt Méid Carn Píob A252 Grád 3

Balla Méideanna ( OD)
.010 1/16" , 1/8" , 3/16"
.020 1/16" , 1/8" , 3/16" , 1/4" , 5/16" , 3/8"
.012 1/8"
.016 1/8" , 3/16"
.028 1/8" , 3/16" , 1/4" , 5/16" , 3/8" , 1/2" , 3/4" , 1" , 1 1/2" , 2"
.035 1/8" , 3/16" , 1/4" , 5/16" , 3/8" , 7/16" , 1/2" , 16" , 5/8" , 3/4" , 7/8" , 1" , 1 1/4" , 1 1/2" , 1 5/8" , 2" , 2 1/4"
.049 3/16" , 1/4" , 5/16" , 3/8" , 1/2" , 16" , 5/8" , 3/4" , 7/8" , 1" , 1 1/8" , 1 1/4" , 1 1/2" , 1 5/8" , 2" , 2 1/4"
.065 1/4" , 5/16" , 3/8" , 1/2" , 16" , 5/8" , 3/4" , 7/8" , 1" , 1 1/4" , 1 1/2" , 1 5/8" , 1 3/4" , 2" , 2 1/2" , 3"
.083 1/4" , 3/8" , 1/2" , 5/8" , 3/4" , 7/8" , 1" , 1 1/4" , 1 1/2" , 1 5/8" , 1 7/8" , 2" , 2 1/2" ,3"
.095 1/2" , 5/8" , 1" , 1 1/4" , 1 1/2" , 2"
.109 1/2" , 3/4" , 1" , 1 1/4" , 1 1/2" , 2"
.120 1/2" , 5/8" , 3/4" , 7/8" , 1" , 1 1/4" , 1 1/2" , 2" , 2 1/4" , 2 1/2" , 3"
.125 3/4" , 1" , 1 1/4" , 1 1/2" , 2" , 3" , 3 1/4"
.134 1"
.250 3"
.375 3 1/2"

Carn píopa cruach A252

ASTM A252 Piling PipeASTM A252 Welded Steel Pipe Piles

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 